Description
English: Stress corrosion cracking of a quench pipe. Material: 1.4541
Date
Source Own work
Author CEphoto, Uwe Aranas
Permission
(Reusing this file)

LOGO-CEphotoUweAranas.png

This photo was created by Uwe Aranas. It is protected by law and is not in the Public Domain. However, it can be used free of charge by everyone under the terms of the license stated below.

  • The requirements to comply with the terms of licence are:
- The image is credited with "Photo by CEphoto, Uwe Aranas" or alternatively with "© CEphoto, Uwe Aranas". If this is not possible due to shortage of space, please contact me first.
- You are required to release the image under the same license.
  • Not required by the license but highly appreciated:
- Set up a weblink to the original image when you use the image in online media: https://commons.wikimedia.org/wiki/File:Stress-Corrosion-Cracking-Quench-Pipe-1.4541-01.jpg
- Send me a specimen copy or a pdf when used in print media or the URL of the website where the image is used.

Please write an email to spam@aranas.de (where you substitute the word spam by cephoto2014), if you

  • need the image in a higher resolution
  • need my postal address for sending a specimen copy
  • have further questions to the terms of licence

No Facebook.svg

This file has been released under a license which is incompatible with Facebook's licensing terms. It is not permitted to upload this file to Facebook.

Attribution
(required by the license)
© CEphoto, Uwe Aranas / 
© CEphoto, Uwe Aranas / 

Upload-problem2.svg

Do not upload new revisions over this file version without my explicit consent. Instead, use the possibility to upload a new version under a new name and tag it as a derivate or extract of this file.

Quality images logo.svg
Quality image

This image has been assessed using the Quality image guidelines and is considered a Quality image.


Licensingedit

I, the copyright holder of this work, hereby publish it under the following license:
w:en:Creative Commons
attribution share alike
This file is licensed under the Creative Commons Attribution-Share Alike 3.0 Unported license.
Attribution: Photo by CEphoto, Uwe Aranas or alternatively © CEphoto, Uwe Aranas
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must attribute the work in the manner specified by the author or licensor (but not in any way that suggests that they endorse you or your use of the work).
  • share alike – If you alter, transform, or build upon this work, you may distribute the resulting work only under the same or similar license to this one.

Photo's description:
Stress corrosion cracking of a quench pipe. Material: 1.4541


Only registered users can post comments. Please login.


EXIF data:
File name stress-corrosion-cracking-quench-pipe-1.4541-01.jpg
Size, Mbytes 3.428306640625
Mime type image/jpeg
Camera manufacturer Canon
Camera model Canon EOS 5D Mark III
Image resolution in width direction 300
Image resolution in height direction 300
Unit of X and Y resolution 2
Exposure time 1/125 sec (0.008)
F number f / 10
Exposure program 1
ISO speed rating 100
Exif version 0230
Lens focal length 100 mm
Date and time original image was generated 2014:07:26 22:50:49
Date and time image was made digital data 2014:07:26 22:50:49
Shutter speed 6.965784
Aperture 6.643856
Exposure bias 0
Maximum lens aperture 3
Metering mode 5
Color space information 1
Focal plane X resolution 3942.5051334702
Focal plane Y resolution 3950.6172839506
Focal plane resolution unit 2
Exposure mode 1
White balance 1
Software used Adobe Photoshop Lightroom 5.3 (Windows)




The pictures at Free-Photos.biz come mainly from Wikimedia Commons or from our own production. The images are either in the public domain, or licensed under free linceses: Free-Photos.biz license, GPL, Creative Commons or Free-Art license. Some very few other photos where uploaded to Free-Photos.biz by our users and released into the public domain or into free usage under another free license (like GPL etc.)

While the copyright and licensing information supplied for each photo is believed to be accurate, Free-Photos.biz does not provide any warranty regarding the copyright status or correctness of licensing terms. If you decide to reuse the images from Free-Photos.biz, you should verify the copyright status of each image just as you would when obtaining images from other sources.


The use of depictions of living or deceased persons may be restricted in some jurisdictions by laws regarding personality rights. Such images are exhibited at Free-Photos.biz as works of art that serve higher artistic interests.

PRIVACY POLICY


By registering your account and/or by subscribing to new and newly rated photographs you agree we may send you the links to photos and we may occasionally share other information with you.

We do NOT disclose your personal data.





christianity portal